Batteries & Electrochemistry · Guide · glidepathscience.org
GuideBatteries & Electrochemistry
Contents
This Guide explains the ideas and equations behind every Walkthrough step, Concept Challenge question and Predict round, in the order a chemistry textbook takes them. Part 1 prepares the Intro track and Part 2 the Advanced track; Part 1 takes about a quarter of an hour to read, Part 2 a little less. Each section ends with a worked example that is not one of the sim’s own problems.
Part 1 · The essentials
Math you’ll need: algebra, powers of ten, and base-10 and natural logarithms.
Chemistry that pushes electrons
Every battery is a chemical reaction in which electrons change hands. In most reactions that transfer happens directly, atom to atom, and the energy released appears as heat. A battery is built so that the electrons cannot go the short way: the substance that gives them up and the substance that takes them are kept apart, and the only path between them is a wire. The electrons flow through the wire, and on the way they can light a lamp, turn a motor or run a phone.
This Guide follows that idea from a strip of zinc in a beaker to the lithium-ion cell in your pocket. It shows how to predict a cell’s voltage from a table, how the voltage is tied to the reaction’s free energy and equilibrium constant, why the voltage falls as a battery runs down, and what a lemon battery really burns.
Voltage and capacity
Two numbers on a battery’s label describe it. The voltage is the energy the battery gives each coulomb of charge it pushes around a circuit: one volt is one joule per coulomb. The capacity, printed in ampere-hours (A·h) or milliampere-hours, is how much charge it can push before it is exhausted. One ampere-hour is one ampere for one hour, which is 3,600 coulombs. The energy stored is the product of the two:
$W = qV$
where $q$ is the charge in coulombs and $V$ the voltage. Multiplying volts by ampere-hours directly gives watt-hours (W·h), a common unit for battery energy; one watt-hour is 3,600 J.
The two numbers come from different places. The voltage is set by the chemistry, which pair of substances reacts, and is the same for a tiny cell and a large one of the same kind. The capacity is set by how much of the reacting material the cell holds: a D cell has far more capacity than an AA cell of the same chemistry, at the same 1.5 V.
Where does that energy come from? From a reaction in which electrons move, which is where the chemistry begins.
Redox reactions and half-cells
A reaction in which electrons are transferred is a redox reaction. The species that loses electrons is oxidized; the species that gains them is reduced. (One way to remember it: oxidation is loss, reduction is gain.) Drop a strip of zinc into blue copper(II) sulfate solution and a coat of copper forms on the zinc while the blue fades:
$Zn(s) + Cu^{2+}(aq) → Zn^{2+}(aq) + Cu(s)$
Each zinc atom gives two electrons to a copper ion. The reaction can be split into two half-reactions, the oxidation $Zn → Zn^{2+} + 2e^−$ and the reduction $Cu^{2+} + 2e^− → Cu$. The sulfate ions are spectators. In the beaker the electrons pass directly at the metal’s surface, so all the energy released warms the solution.
To make the electrons do work, put each half-reaction in its own half-cell: zinc in zinc sulfate in one beaker, copper in copper sulfate in another. Join the two metals with a wire and the two solutions with a salt bridge, a tube of a salt solution such as potassium nitrate. Now zinc atoms give up electrons in one beaker, the electrons travel through the wire, and copper ions take them in the other. The bridge is essential: as zinc ions pour into the first solution and copper ions leave the second, the solutions would become charged and stop the reaction at once. Ions drifting through the bridge (positive ions toward the copper, negative ions toward the zinc) keep both neutral. Electrons travel only in the wire; in the solutions and the bridge, charge is carried by ions.
Two half-cells joined this way make a galvanic cell, and its two electrodes have names.
Anode, cathode and cell notation
The electrode where oxidation happens is the anode; the electrode where reduction happens is the cathode. In the zinc–copper cell, called the Daniell cell, zinc is the anode and copper the cathode. Oxidation at the anode leaves electrons behind on the metal, so in a galvanic cell the anode is the negative terminal and the cathode the positive one. Electrons flow out of the anode, through the wire, into the cathode.
Chemists write a cell in a shorthand called cell notation. The anode goes on the left and the cathode on the right; a single vertical bar marks each boundary between phases, and a double bar marks the salt bridge:
$Zn(s) | Zn^{2+}(aq) ‖ Cu^{2+}(aq) | Cu(s)$
Read left to right, the notation runs from the oxidation to the reduction. A common slip is to reverse it, or to write a single bar where the salt bridge belongs.
Which metal is oxidized is not a guess: a table decides it, and gives the voltage too.
Standard reduction potentials
Each half-cell has a tendency to be reduced, measured as its standard reduction potential $E°$. Because only differences of potential can be measured, one half-cell is chosen as the zero: the standard hydrogen electrode, platinum in 1 M acid with hydrogen gas at 1 bar, whose reaction $2H^+ + 2e^− → H_2$ has $E°$ = 0 by definition. Every other couple is measured against it at standard conditions (1 M solutions, 1 bar gases, usually 25 °C). The more positive $E°$, the more readily the couple is reduced: silver ions (+0.7996 V) and copper ions (+0.337 V) sit high on the table, zinc (−0.7618 V) and magnesium (−2.372 V) low.
In a cell, the couple higher on the scale is reduced (the cathode) and the lower one is oxidized (the anode). The standard cell potential is the difference:
$E°_{cell} = E°_{cathode} − E°_{anode}$
A cell that runs has a positive $E°_{cell}$. One rule causes more mistakes than any other: a potential is energy per coulomb, so it does not change when a half-reaction is multiplied to balance the electrons. Doubling a reaction doubles both the charge and the energy, and leaves their ratio alone. Never multiply an $E°$ by a coefficient.
A positive cell potential means the reaction runs on its own. That statement is about free energy.
Free energy and the equilibrium constant
A cell’s voltage is its reaction’s free energy, per coulomb. If $n$ moles of electrons move for each mole of reaction, the charge is $nF$, where $F$ = 96,485 C/mol is Faraday’s constant, the charge on a mole of electrons. The most electrical work the reaction can do is that charge times the voltage, and it equals the decrease in Gibbs free energy:
$ΔG° = −nFE°_{cell}$
A positive $E°_{cell}$ gives a negative $ΔG°$: the reaction is spontaneous. Reverse the reaction and both signs flip. Volts times coulombs are joules, so $ΔG°$ comes out in joules per mole of reaction.
The standard free-energy change also sets the equilibrium constant, $ΔG° = −RT\ln K$. Putting the two together gives $E°_{cell} = (RT/nF)\ln K$. At 25 °C the combination $(RT/F)\ln 10$ is 0.05916 V, so in base-10 logarithms
$\log_{10}K = nE°/(0.05916\ \text{V})$
Every 0.05916 V of cell potential per electron is another factor of ten in $K$. That is why a cell of only a volt or so has an enormous equilibrium constant: at equilibrium there is essentially none of the limiting reactant left.
Standard conditions are a starting point. Real cells have other concentrations, and their voltage changes as they run.
The Nernst equation and the dead battery
Away from standard conditions, the cell potential depends on the reaction quotient $Q$, the same ratio of concentrations that appears in an equilibrium constant but with the concentrations as they are now. Solids do not appear in $Q$. For the Daniell cell, $Q = [Zn^{2+}]/[Cu^{2+}]$. The Nernst equation gives the voltage:
$E = E° − (0.05916\ \text{V}/n)\log_{10}Q$
at 25 °C. More product or less reactant makes $Q$ larger and the voltage smaller; the reverse raises it. Because the change goes with the logarithm, it is modest: for two electrons, a tenfold change in $Q$ moves the voltage by only 0.0296 V.
Now let the cell run. Zinc dissolves and copper plates out, so $[Zn^{2+}]$ rises, $[Cu^{2+}]$ falls, $Q$ climbs and $E$ falls. The voltage reaches zero exactly when $Q$ equals $K$: the reaction has reached equilibrium, $ΔG$ = 0, and no more work can be had. That is a dead battery. It is not that every reactant is gone: in the Daniell cell plenty of zinc is usually left, and the copper ions have fallen to their tiny equilibrium concentration. The standard potential $E°$ never changes as a cell runs; it is $E$, the actual voltage, that falls.
The same ideas explain a lemon battery, and what happens when a battery is recharged.
The lemon, and recharging
Push a galvanized nail (coated with zinc) and a copper strip into a lemon and a meter reads about 0.9 V. It is tempting to think the lemon is the battery, but the lemon only supplies the electrolyte. The zinc is oxidized, $Zn → Zn^{2+} + 2e^−$, and the juice’s acid supplies hydrogen ions that take the electrons at the copper, $2H^+ + 2e^− → H_2$. The overall reaction is $Zn + 2H^+ → Zn^{2+} + H_2$: the zinc is the fuel, and the copper is not used up at all. A lemon cell also has a large internal resistance, so although its voltage is respectable, it can deliver well under a milliamp: three in series light a red LED only faintly.
A battery can be recharged only if its reaction can be driven backward. A charger connected + to + and − to −, at a voltage higher than the cell’s own, pushes current the other way through the cell, so the products are turned back into reactants: in the Daniell cell, zinc ions are plated back as zinc and copper dissolves. A cell driven by an outside supply is an electrolytic cell. The anode is still where oxidation happens, but now it is the positive electrode (copper, in the recharged Daniell cell) and the cathode is negative. “The anode is negative” is true only for a galvanic cell.
Part 2 · Going further
Math you’ll need: everything in Part 1, natural logarithms, and the idea of a derivative (one section uses $dE°/dT$).
The EMF as thermodynamics
At constant temperature and pressure, the most work a reaction can do, other than pushing back the atmosphere, is $−ΔG$. A cell run reversibly, with an opposing voltage just below its own so that the current is vanishingly small, delivers exactly that: $w_{max} = nFE$. The rest of the reaction’s enthalpy change is heat exchanged with the surroundings even in the reversible cell, $q_{rev} = TΔS$. In a beaker the same reaction turns all of $ΔH$ into heat. This is why a cell is the cleanest way to measure a reaction’s free energy.
A cell also measures entropy. Since $(∂ΔG/∂T)_p = −ΔS$ and $ΔG° = −nFE°$,
$ΔS° = nF\,dE°/dT$
A cell whose standard potential falls as it warms has a negative $ΔS°$; one whose potential rises has a positive one. With $ΔG°$ and $ΔS°$ in hand, $ΔH° = ΔG° + TΔS°$ follows, so a voltmeter and a thermometer together give all three. For the Daniell cell the potential falls by about 0.11 mV per kelvin, a small effect that is easy to measure.
The temperature coefficient of a single couple, measured against the hydrogen electrode, comes from the standard entropies of its species. This sim uses those values and treats $ΔS°$ as constant over 0–80 °C, so each $E°$ changes linearly with temperature.
Deriving Nernst, and its slope
The Nernst equation comes straight from thermodynamics. The free-energy change at any composition is $ΔG = ΔG° + RT\ln Q$. Divide through by $−nF$, using $ΔG = −nFE$ and $ΔG° = −nFE°$:
$E = E° − (RT/nF)\ln Q$
The scale is set by $RT/F$, which at 25 °C is 25.69 mV. Per factor of ten in $Q$ the voltage changes by $(RT/nF)\ln 10$, 59.16 mV for one electron at 25 °C. The slope is proportional to the absolute temperature, which is why the Part 1 form with 0.05916 V holds only at 25 °C. The glass pH electrode in the Acid–Base Titration Lab responds to hydrogen ions with this same slope, 59.16 mV per pH unit at 25 °C, and pH meters correct it for temperature.
Concentration cells and activities
A cell can be made from one metal in two solutions of its ion at different concentrations. Its $E°$ is zero, yet it has a voltage, because $Q$ is not 1: $E = (0.05916\ \text{V}/n)\log_{10}(c_{high}/c_{low})$ at 25 °C. Metal dissolves into the dilute side, which is therefore the anode, and plates out of the concentrated side, until the two concentrations are equal. The whole driving force is the mixing of the two solutions; nerve cells use the same idea across their membranes.
Strictly, the Nernst equation takes activities, not concentrations: $a = γc$, where the activity coefficient $γ$ is less than 1 because each ion is surrounded by a cloud of oppositely charged ions that shields it. In dilute solution the Debye–Hückel limiting law gives, at 25 °C,
$\log_{10}γ = −0.509\,z^2\sqrt{I}$
with $z$ the ion’s charge and the ionic strength
$I = \tfrac12\sum c_iz_i^2$
which counts every ion in the solution. Doubly charged ions are affected four times as strongly as singly charged ones. The limiting law holds only below about $I$ = 0.01 M; at higher ionic strength measured coefficients are used. This sim’s Sandbox uses ideal concentrations throughout.
The salt bridge and junction potentials
Wherever two different solutions meet, ions diffuse across the boundary, and if the positive and negative ions move at different speeds a little charge separates. The result is a liquid-junction potential, typically a few to a few tens of millivolts, which adds to whatever the voltmeter reads. Salt bridges are filled with concentrated potassium chloride or potassium nitrate because their two ions have nearly the same mobility: they carry almost all the current at each end of the bridge and separate almost no charge, so the junction potentials stay at a few millivolts and largely cancel. This sim sets them to zero.
Cells under load: resistance and overpotential
A cell’s open-circuit voltage is its EMF $E$. Once it delivers a current $I$, two things lower the voltage at its terminals. The first is its internal resistance $r$, from the solutions and the bridge or separator: on a load $R$, the current is $I = E/(R + r)$ and the terminals read
$V = E − Ir$
The more current drawn, the more voltage is lost inside, as heat.
The second is overpotential: driving an electrode reaction faster than its natural exchange rate takes extra voltage. At high current densities the Tafel equation describes it,
$η = b\log_{10}(i/i_0)$
where $b$ is the Tafel slope (often 0.03–0.12 V per decade) and $i_0$ the exchange current density, large for a good catalyst and small for a poor one. Each tenfold increase in current costs another $b$. Hydrogen evolution on copper is slow, so a lemon cell loses voltage to overpotential as soon as it delivers current. The lemon also illustrates the limits of the ideal table: zinc against a hydrogen electrode at the juice’s pH of about 2.2 should give only about 0.72 V with 1 mM Zn²⁺ (0.63 V at 1 M), yet lemon cells read nearer 0.9 V, because the copper’s potential is a mixed potential, with dissolved oxygen reduced there as well.
Real batteries
A cell’s capacity is set by its limiting reactant: the charge it can pass is $nF$ times the moles of that reactant. At a steady current the run time follows directly,
$t = nFcV/I$
for a limiting ion of concentration $c$ in a volume $V$. The voltage, meanwhile, hardly changes while both electrodes have plenty of material, because the Nernst term is logarithmic, and then falls steeply as the limiting reactant runs out. A real discharge curve looks the same: nearly flat, then a knee and a drop to the cutoff voltage below which the device stops.
Each chemistry’s voltage comes from its pair of reactions. An alkaline cell (zinc and manganese dioxide) gives about 1.5 V; a lead–acid cell, whose reactions $PbO_2 + SO_4^{2−} + 4H^+ + 2e^− → PbSO_4 + 2H_2O$ (+1.69 V) and $PbSO_4 + 2e^− → Pb + SO_4^{2−}$ (−0.3505 V) give 2.04 V, is rechargeable; a lithium-ion cell gives 3.6–3.7 V on average. Water limits the others: above about 1.23 V water itself can be split, and only slow electrode kinetics lets lead–acid exceed it. Lithium-ion cells use an organic electrolyte with no water, which lets them exploit lithium’s very negative potential (−3.04 V). Drawing more current lowers the whole curve by $Ir$ and reaches the cutoff sooner, so less of the capacity is used.
Electrolysis and Faraday’s law
In an electrolytic cell an outside supply drives a reaction that would not run on its own: plating metal, refining copper, making aluminum or chlorine, or recharging a battery. Michael Faraday found that the amount of substance produced is proportional to the charge passed. A current $I$ for a time $t$ carries $q = It$; that is $q/F$ moles of electrons, and each metal ion needs $n$ of them, so the mass deposited is
$m = ItM/(nF)$
with $M$ the molar mass. The same charge plates twice as many moles of a +1 ion as of a +2 ion. Time must be in seconds, and $n$ is the ion’s charge.
Reference
Common mistakes
Part 1
- Thinking electrons travel through the salt bridge: in solutions, charge is carried by ions.
- “The anode is always negative”: it is negative in a galvanic cell, positive in an electrolytic one; the anode is wherever oxidation happens.
- Multiplying a standard potential by a coefficient: potentials are energy per charge and never scale with the reaction.
- Subtracting the wrong way, or adding: $E°_{cell} = E°_{cathode} − E°_{anode}$, and a working cell’s is positive.
- Forgetting $n$, or the minus sign, in $ΔG° = −nFE°$; giving $\ln K$ for $\log_{10}K$.
- Getting the Nernst sign backward: larger $Q$ means a lower voltage. Solids never appear in $Q$.
- Thinking a dead battery has no reactants left: it has reached equilibrium, $Q = K$.
- Thinking the lemon is the battery: the zinc is the fuel; the lemon is the electrolyte.
- Confusing voltage with capacity: voltage is set by the chemistry, capacity by the amount of material; and 1 A·h is 3,600 C.
Part 2
- Taking $−ΔH$ as the maximum work: it is $−ΔG$; $TΔS$ is heat even in a reversible cell.
- Using the 25 °C slope at other temperatures, or degrees Celsius in $RT/F$.
- Making the concentrated side of a concentration cell the anode: the dilute side is oxidized.
- Forgetting $z^2$, or one of the ions, in the Debye–Hückel law; using it above $I$ ≈ 0.01 M.
- Quoting $E$ for the terminal voltage of a cell delivering current: it is $E − Ir$, less any overpotential.
- Minutes instead of seconds, or the wrong $n$, in Faraday’s law.
Equation sheet
| Part 1 | |
|---|---|
| energy | $W = qV$, with 1 A·h = 3,600 C |
| cell potential | $E°_{cell} = E°_{cathode} − E°_{anode}$ |
| free energy | $ΔG° = −nFE°_{cell}$ |
| equilibrium | $\log_{10}K = nE°/(0.05916\ \text{V})$ |
| Nernst, 25 °C | $E = E° − (0.05916\ \text{V}/n)\log_{10}Q$ |
| Part 2 | |
|---|---|
| Nernst | $E = E° − (RT/nF)\ln Q$ |
| entropy | $ΔS° = nF\,dE°/dT$ |
| ionic strength | $I = \tfrac12\sum c_iz_i^2$ |
| Debye–Hückel | $\log_{10}γ = −0.509\,z^2\sqrt{I}$ |
| under load | $V = E − Ir$ |
| Tafel | $η = b\log_{10}(i/i_0)$ |
| Faraday | $m = ItM/(nF)$ |
| run time | $t = nFcV/I$ |
$F$ = 96,485 C/mol (Faraday’s constant); $R$ = 8.314 J/(mol·K); $T$ in kelvin; $n$ the moles of electrons per mole of reaction; $Q$ and $K$ the reaction quotient and equilibrium constant; $r$ the internal resistance; $γ$ the activity coefficient; $z$ an ion’s charge; $η$ the overpotential; $M$ the molar mass; $c$ and $V$ a limiting ion’s concentration and volume.
Sources and further reading
OpenStax, Chemistry 2e, by Paul Flowers, Klaus Theopold, Richard Langley and William R. Robinson, Chapter 17, “Electrochemistry” (§17.1–17.7), and Appendix L, “Standard Electrode (Half-Cell) Potentials”, CC BY-NC-SA 4.0, openstax.org: the Intro track follows its order and notation, and every standard potential here is Appendix L’s. Faraday’s constant and the gas constant are the exact values of the 2019 SI. The temperature coefficients come from standard entropies in the NBS tables of chemical thermodynamic properties. The Field Manual (H) describes the model and what it leaves out; the Lemon Lab and Battery Shop values are typical, not measured on any particular fruit or product.
Batteries & Electrochemistry v1.0 · © 2026 Dr. David Meier · CC BY-NC-SA 4.0 · glidepathscience.org